Tiangang® HS-788

Hindered amine light stabilizer (hals) · HS-788
synergistic mixture of high molecular weight light stabilizers. It is a highly effective radical scavenger belonging to the Hindered Amine Light Stabilizers (HALS) family of stabilizers. It is a versatile UV stabilizer with high extraction resistance
In one sentence: A synergistic blend of oligomeric hindered amines balancing diffusion and retention across molecular weights, for films and fibres.
- Film, flat yarn, nonwoven dosage: 0.1 – 0.5% (source: recommended dosing table on this page)
- Injection mouldings, medium/thick-wall dosage: 0.3 – 1.0% (source: recommended dosing table on this page)
- Fibre and monofilament dosage: 0.3 – 0.8% (source: recommended dosing table on this page)
What it is
Tiangang® HS-788 is a hindered amine light stabilizer (HALS). HALS trap the radicals formed when a polymer photo-oxidises and regenerate in the process, so the protection window is longer than that of a UV absorber, which is consumed as it works.
Technical data
| Chemical name | Hindered amine derivatives |
| Description | Tiangang® HS-788 is a synergistic mixture of high molecular weight light stabilizers. It is a highly effective radical scavenger belonging to the Hindered Amine Light Stabilizers (HALS) family of stabilizers. It is a versatile UV stabilizer with high extraction resistance, low fading and low pigment interaction, and particularly well suited for LDPE, LLDPE, HDPE films, tapes and thick sections and for PP in fibers and films. It is also the product of choice for thick sections where indirect food contact approval is required. |
| Appearance | Softening range oC | Weight loss - 10%, oC | Flash point oC | |
| Tiangang® HS-788 FD | Yellowish pastilles | 105~120 | > 350 | > 192 |
| Tiangang® HS-788 LD | Yellowish powders |
| Tiangang® HS-788 FD/LD | The use of proper protective equipment is recommended. Excess exposure to the product should be avoided. Wash thoroughly after handling. Store the product in a cool, dry, well-ventilated area away from incompatible materials. |
| Disclaimer | The information supplied is presented in good faith and has been derived from sources believed to be reliable. Since conditions of use are beyond our control, all risks are assumed by the user. No representation is expressed or implied, and nothing herein shall be construed as permission or recommendation to practice a patented invention without license. |
Where it is used, and at what loading
Suitable for polyolefins (PP, PE), polyurethane, polyamide, polyacetal and polyester. Thin and thick parts call for different grades: thin sections suffer from volatilisation and migration, thick sections from surface bloom.
| Film, tape, nonwoven | 0.1 – 0.5% |
|---|---|
| Injection moulded and thick-wall parts | 0.3 – 1.0% |
| Fibre and monofilament | 0.3 – 0.8% |
Figures above are typical industry ranges, not guaranteed values. The actual loading depends on wall thickness, design life and the other additives in the system, and should be established by a loading ladder on the real formulation.
Choosing between similar grades
Three things decide the choice for HS-788: molecular weight and volatility, basicity, and compatibility with the other components in the system. A synergistic blend of oligomeric HALS covering both diffusion speed and retention; a single high-MW grade acts too slowly in thin sections.
Frequently asked questions
Is this grade meant for thin or thick parts?
It depends on molecular weight and migration tendency. Low-MW grades diffuse quickly and act early but volatilise and migrate over time; high-MW grades (HS-950, HS-362, BW-10LD) suit long-service outdoor parts. Tiangang offers both, so the choice follows wall thickness and design life.
Is it worth combining with a UV absorber?
Yes, they cover different stages. The UV absorber shields incoming UV energy; the HALS scavenges radicals that have already formed. Agricultural film, automotive exterior and PV backsheet usually need both to reach their design life.
What happens if the loading is too high?
Beyond the compatibility limit the additive blooms to the surface, which wastes material and harms appearance and print adhesion. Protection also stops scaling linearly. Our practice is a loading ladder on the actual system, then fix the cost-performance knee.
The figures and guidance above follow Tiangang's published technical material and common industry practice. For a specific formulation, refer to the batch COA and the technical agreement between the parties.
Certifications
- National High-Tech Enterprise
- Vice Chairman Unit, China Plastics Processing Industry Association (CPPIA)
- Vice Chairman Unit, Agricultural Plastics Branch, China Agricultural Plastics Application Technology Society
- Member, Ageing Methods Subcommittee, National Technical Committee on Plastics (SAC/TC15/CS5)
- Member, Society of the Plastics Industry (SPI), USA
Recommended Products
Products
UV Absorbers
400-094-4362
- Tiangang elected Executive Deputy Director Unit of CPPIA Agricultural Film Committee
- Tiangang wins Leading Award at Beijing TV Innovation Institute finals
- Tiangang concludes CHINAPLAS 2023 on a high note
- First industry-academia-research base in Weishanzhuang Town lands at Tiangang
- Tiangang-Tinaco BUCT scholarship award ceremony 2021-2022